A131 AH32 high Strength Chemical Composition
Grade
The Element Max (%)
C
Si
Mn
P
S
Al
N
A131 AH32
0.18
0.1-0.50
0.90-1.6
0.035
0.035
0.015
 
Nb
V
Ti
Cu
Cr
Ni
Mo
0.02-0.05
0.05-0.10
0.02
0.35
0.2
0.4
0.08

 
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%
 
 

A131 AH32 high strength property
Grade
 
Mechanical Property
Charpy V Impact Test
Thickness
Yield
Tensile
Elongation
Degree
Energy 1
Energy 2
A131 AH32
mm
Min Mpa
Mpa
Min %
0
J
J
t50
315
440-590
19%
17
25
50t70
315
440-590
19%
19
28
70t100
315
440-590
19%
23
34
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
 
 
 
 

Equivalent steel grade of A131 AH32
NV A32
GL-A32
LR/AH32
BV/AH32
CCS/A32
K A32
R A32
RI/A32

 
 
 
 
If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.
 
 
 
 

Tags: A131 AH32  A131 Grade AH32  AH32 steel  

0 Comments, 0 Trackbacks