A131 DH32 STEEL PLATE
Gangsteel is specialized in supplying A131 high strength steel plate in A131 Grade DH32. For more information of GradeDH32 steel plate, please check them in following:
A131 DH32 high Strength Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
A131 DH32 | 0.18 | 0.1-0.50 | 0.90-1.6 | 0.035 | 0.035 | 0.015 | |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
A131 DH32 high strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
A131 DH32 | mm | Min Mpa | Mpa | Min % | -20 | J | J |
t≤50 | 315 | 440-590 | 19% | 17 | 25 | ||
50<t≤70 | 315 | 440-590 | 19% | 19 | 28 | ||
70<t≤100 | 315 | 440-590 | 19% | 23 | 34 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Equivalent steel grade of A131 DH32 | |||||||
NV D32 | GL-D32 | LR/DH32 | BV/DH32 | CCS/D32 | K D32 | R D32 | RI/D32 |