A131 Grade EH32 | A131 EH32 STEEL PLATE
2011年11月16日 by admin
Gangsteel is specialized in supplying A131 high strength steel plate in A131 Grade DH32. For more information of GradeEH32 steel plate, please check them in following:
A131 EH32 high Strength Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
A131 EH32 | 0.18 | 0.1-0.50 | 0.90-1.6 | 0.035 | 0.035 | 0.015 | |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
A131 EH32 high strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
A131 EH32 | mm | Min Mpa | Mpa | Min % | -40 | J | J |
t≤50 | 315 | 440-590 | 19% | 17 | 25 | ||
50<t≤70 | 315 | 440-590 | 19% | 19 | 28 | ||
70<t≤100 | 315 | 440-590 | 19% | 23 | 34 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Equivalent steel grade of A131 EH32 | |||||||
NV E32 | GL-E32 | LR/EH32 | BV/EH32 | CCS/E32 | K E32 | R E32 | RI/E32 |