New Products /back


A131 EH40 | A131 Grade EH40 STEEL PLATE

2011年11月16日 by admin

 

               
 
Gangsteel is specialized in supplying A131 high strength steel plate in A131 Grade EH40. For more information of GradeEH40 steel plate, please check them in following:
 

A131 EH40 high Strength Chemical Composition
Grade
The Element Max (%)
C
Si
Mn
P
S
Al
N
A131 EH40
0.18
0.1-0.50
0.90-1.6
0.035
0.035
0.015
 
Nb
V
Ti
Cu
Cr
Ni
Mo
0.02-0.05
0.05-0.10
0.02
0.35
0.2
0.4
0.08

 
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%
 
 

A131 EH40 high strength property
Grade
 
Mechanical Property
Charpy V Impact Test
Thickness
Yield
Tensile
Elongation
Degree
Energy 1
Energy 2
A131 EH40
mm
Min Mpa
Mpa
Min %
-40
J
J
t50
390
510-650
22%
20
30
50t70
390
510-650
22%
-
-
70t100
390
510-650
22%
-
-
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
 
 
 
 

Equivalent steel grade of A131 EH40
NV E40
GL-E40
LR/EH40
BV/EH40
CCS/E40
K E40
R E40
RI/E40

 
 
 
 
If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.
 
 
 
 

Tags: A131 Grade EH40  A131 EH40  