A131 Grade FH36 | A131 FH36 STEEL PLATE
2011年11月21日 by admin
Gangsteel is specialized in supplying A131 high strength steel plate in A131 Grade FH36. For more information of GradeFH36 steel plate, please check them in following:
A131 FH36 high Strength Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
A131 FH36 | 0.16 | 0.1-0.50 | 0.90-1.6 | 0.025 | 0.025 | 0.015 | 0.009 |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
A131 FH36 high strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
A131 FH36 | mm | Min Mpa | Mpa | Min % | -60 | J | J |
t≤50 | 355 | 490-620 | 22% | 17 | 25 | ||
50<t≤70 | 355 | 490-620 | 22% | 20 | 30 | ||
70<t≤100 | 355 | 490-620 | 22% | 25 | 37 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Equivalent steel grade of A131 FH36 | |||||||
NV F36 | GL-F36 | LR/FH36 | BV/FH36 | CCS/F36 | K F36 | R F36 | RI/F36 |