A131 GRADE D STEEL PLATE

2011年11月21日 by admin

 

                           
 
Gangsteel is specialized in supplying A131 general strength steel plate in A131 Grade D For more information of Grade D Steel plate, please check them in following:
 
 

A131 GRADE D general Strength Chemical Composition
Grade
The Element Max (%)
C
Si
Mn
P
S
C+Mn/6
A131 GRADE D
0.21
0.10-0.35
0.60
0.035
0.035
0.40

Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%
 
 

A131 GRADE D high strength property
Grade
 
Mechanical Property
Charpy V Impact Test
Thickness
Yield
Tensile
Elongation
Degree
Energy 1
Energy 2
A131 GRADE D
mm
Min Mpa
Mpa
Min %
-20
J
J
t50
235
400-520
21%
14
20
50t70
235
400-520
21%
17
25
70t100
235
400-520
21%
20
30
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
 
 
 
 

Equivalent steel grade of A131 GRADE D
NV D
GL-D
LR/D
BV/D
CCS/D
K D
R D
RI/D

 
 
 
 
If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.
 
 
 
 
 
 