A131 GRADE E STEEL PLATE
2011年11月15日 by admin
A131 GRADE E STEEL PLATE
Gangsteel is specialized in supplying A131 general strength steel plate in A131 Grade E For more information of Grade E Steel plate, please check them in following:
A131 GRADE E general Strength Chemical Composition | ||||||
Grade | The Element Max (%) | |||||
C | Si | Mn | P | S | C+Mn/6 | |
A131 GRADE E | 0.21 | 0.10-0.35 | 0.70 | 0.035 | 0.035 | 0.40 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
A131 GRADE E high strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
A131 GRADE E | mm | Min Mpa | Mpa | Min % | -40 | J | J |
t≤50 | 235 | 400-520 | 21% | 14 | 20 | ||
50<t≤70 | 235 | 400-520 | 21% | 17 | 25 | ||
70<t≤100 | 235 | 400-520 | 21% | 20 | 30 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Equivalent steel grade of A131 GRADE E | |||||||
NV D | GL-D | LR/D | BV/D | CCS/D | K D | R D | RI/D |
If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.