A131 FH32 | A131 Grade Fh32 STEEL PLATE
2011年11月21日 by admin
Gangsteel is specialized in supplying A131 high strength steel plate in A131 Grade DH32. For more information of GradeFH32 steel plate, please check them in following:
A131 FH32 high Strength Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
A131 FH32 | 0.16 | 0.1-0.50 | 0.90-1.6 | 0.025 | 0.025 | 0.015 | 0.009 |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
A131 FH32 high strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
A131 FH32 | mm | Min Mpa | Mpa | Min % | -60 | J | J |
t≤50 | 315 | 440-590 | 19% | 17 | 25 | ||
50<t≤70 | 315 | 440-590 | 19% | 20 | 30 | ||
70<t≤100 | 315 | 440-590 | 19% | 25 | 37 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Equivalent steel grade of A131 FH32 | |||||||
NV F32 | GL-F32 | LR/FH32 | BV/FH32 | CCS/F32 | K F32 | R F32 | RI/E32 |
If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.