New Products /back


A202 Grade A steel plate

2013年7月15日 by admin

ASTM A202 GrA|A202 Grade A steel plate

 

ASTM A202 standard specification for pressure vessel plates, alloy steel, chromium-manganese-silicon

 

ASTM A202 plates are normally supplied in the as-rolled condition. The plates may be ordered normalized or stress relieved, or both.

 

Our plates including A202 Grade A come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.

 

 

Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2 | S3 | S4.1
S5 | S6 | S7 | S8 | S9| S11 | S12 | S14 | S17

 

Dimension: Thickness: 6MM to 300MM,

Width: 1500mm to 4050mm,

Length: 3000mm to 15000mm

A202 Grade A Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

A202 grade A

0.17

0.54-0.90

0.97-1.52

0.035

0.035

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Grade

 A202 Grade A Mechanical Property

Thickness

Yield

Tensile

Elongation

A202 grade A

mm

Min Mpa

Mpa

Min  %

6-50

310

515-655

19%

50-100

310

515-655

16%

Shipbuilding steel plate| Alloy steel plates| High strength plate| Carbon steel plate| Stainless steel plate

 

Equivalent steel grade of A202 grade A

Europe

Belgium

Germany

France

Italy

Sweden

India

Japan

 

 

E St E315

18 MD 4.05

16 Mo 6

22.16.04

 

450M

 

Related steel grades: A202 Grade A| A202 Grade B

 

Gangsteel is specialized in supplying boiler and pressure vessel steel plate, mainly dealing with specification standard plates in ASTM A285, ASTM A537, ASTM A516, ASTM A515, ASTM A514, ASTM A662, ASTM A387, ASTM A517, ASTM A203, ASTM A202, ASTM A203, SA302, JIS G3115, JIS G3103, EN 10028-2, EN 10028-3, EN 10028-5, EN 10028-6, and thickness can be up to 300mm.

 

To find out more about A202 Gr.A or other boiler and pressure vessel steel plate, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.

 

Tags: A202 Grade A  A202 Gr.A  ASTM A202 Gr.A  

0 Comments, 0 Trackbacks