A204 Grade B STEEL PLATE
2013年7月15日 by admin
ASTM A204 standard specification for Pressure Vessel Plates, Alloy Steel, Molybdenum .
ASTM A204 Grade B is used in fabricators serving industry, especially in the oil, gas and chemical supply markets.
Our plates including A204 Grade B come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.
Supplementary Technology: HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2 | S3 | S4.1
S5 | S6 | S7 | S8 | S9| S11 | S12 | S14 | S17
Dimension: Thickness:
Width:
Length:
Gangsteel is specialized in supplying ASTM A204 steel plate in A204 Grade B. For more information of A204 Grade B steel plates, please check them in following:
A204 Grade B Chemical Composition | |||||
Grade | The Element Max (%) | ||||
C | Si | Mn | P | S | |
A204 Grade B | 0.20-0.27 | 0.13-0.45 | 0.90-0.98 | 0.035 | 0.035 |
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Mechanical Property of A203 Grade A steel plate | A204 Grade B |
Tensile strength, kis [MPa] | 70-90 [485-620] |
Yield strength, min, kis [MPa] | 40 [275 |
Elongation in 8 in. [200 mm], min, % | 17 |
Elongation in 2 in. [50 mm], min, % | 21 |
Shipbuilding steel plate | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate
Equivalent steel grade of A204 Grade B | |||||||
| | | | | | | |
| | | 15 CD 4.05 | | | | |
Related Grade: A204 Grade B | A204 Grade A | A204 Grade C
Gangsteel is specialized in supplying boiler and pressure vessel steel plate, mainly dealing with specification standard plates in ASTM A285, ASTM A537, ASTM A516, ASTM A515, ASTM A514, ASTM A662, ASTM A387, ASTM A517, ASTM A203, ASTM A202, ASTM A203, SA302, JIS G3115, JIS G3103, EN 10028-2, EN 10028-3, EN 10028-5, EN 10028-6, and thickness can be up to 300mm.
To find out more about A204 Gr.B or other boiler and pressure vessel steel, and to receive a competitive quotation for supply of this material, please CLICL HERE to contact us.
Tags: A204 Gr. B A204 Grade B ASTM A204 GRB
0 Comments, 0 Trackbacks