A537 Class 3 steel plate
 
 
Adopt standard: A 537 ASTM
Sell steel grade: A537 Class 1 steel grade, A537 Class 2 steel grade, A537 Class 3 steel grade
 
 
A537 Class 3 steel grade
 
 
Steel plate A 537 CL3 is a quenched and tempered steel material, the same with A 537 CL2 in heat treatment.
 
Although the A 537 CL3 only yields strength lower than A 573 CL2, the two grade have a little different in price. A 537 cl3 quenched and tempered temperature is 620, and A 537 cl2 is 595.

A 537 CL3 steel plate max thickness is 150mm according to standard of A 537/ SA537 standard. But if customers more thickness above 150mm, our mill also could produce them. This is our advantage in manufacture.
 
Gangsteel supplies A 537 Class 3 on the base of customer’s request. We could do S1, S2, S3, S4.1, S5, S6, S7, S8, S11, S12,S14 AND S17 supplementary requirements.
Welcome to visit our mill in China for a long steel business cooperation.
 
About A 537 CL 3 detail information,please check technical date in following.
 
 
The Chemical is max composition of product analysis:
 

Grade
C %
Si %
Mn %
P %
S %
Cu %
Ni %
Cr %
Mo %
A 537 CL3
0.240
0.13-0.55
0.64-1.46
0.035
0.035
0.380
0.280
0.290
0.090

 
 
 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
A537CL3
8mm-65mm
Min 380Mpa
550-690Mpa
22%
66mm-100mm
Min 345Mpa
515-655Mpa
22%
101mm-150mm
Min 275Mpa
485-620Mpa
20%

 
 
 