 A387 Grade 11 Cl1,A387 Grade 11 Cl2,A387 Grade 22 Cl1,A387 Grade 22 Cl2 steel plate

 

 

A 387 steel specification covers chromium and Molybdenum pressure vessel plate in grade A 387 Grade 11 Class 1, A387 Grade 11 Class 2, A387 Grade 22 Class 1, A387 Grade 22 Class 2, steel

 

 1. Steel Grade:
A 387 Grade 2 Class 1, A 387 Grade 2 Class 2, A 387 Grade 12 Class 1, A 387 Grade 12 Class 2, A 387 Grade 11 Class 1, A 387 Grade 11 Class 2, A 387 Grade 22 Class 1, A 387 Grade 22 Class 2, A 387 Grade 22L Class 1, A 387 Grade 21 Class 1, A 387 Grade 21 Class 2, A 387 Grade 21L Class 1, A 387 Grade 5 Class 1, A 387 Grade 5 Class 2, A 387 Grade 9 Class 1, A 387 Grade 9 Class 2, A 387 Grade 91 Class 2 and A 387 Grade 911 Class 2.

 2. Supply steel Size: Thickness: 8mm to 200mm, Width: 1500mm to 4200mm, Length: 4000mm to 18000mm
3. Adopt Standard:  ASTM A 387 and ASME SA 387
4. Heat Treatment: Hot Rolled, CR, Normalized, Quenched, Tempering, TMCP, Electroslag Remelting Technical, HIC test.
5. Delivery Time: 30-40days
6. Payment Item: 30% TT, or LC and TT.
7. Steel Services: Cutting, Painting, Ball blast, Pretreatment , and The third party inspection in DNV, BV, LR, GL, ABS, CCS , CE Mark, TUV, ISO, and others in super thick ship steel plate.

 

Henan Gang Iron and Steel Co Ltd, is a largest agent of Wuyang mill in HBIS. We have many stock in steel plate stock in shanghai and Wuyang warehouse.


Gangsteel is specialized in super thick boiler steel plate and cooperated with ABS, BV, DNV, CCS, GL, LR, KR, NK, and RINA Classification Society to approve the super thickness plate to 200mm now.

 

Besides that, Gangsteel Boss is a manufacture manger, so we could promise the delivery time and the competitive price comparing with other company.

 

We sincerely hope new and old customers come to visit our mill and inquiry from Gangsteel.

 

Henan Gang Iron and Steel Co., Ltd

Tel: 86-0371-88884766  Fax: 86-0371-88884766
Cell: 86-15226033579
Email: olina@gangsteel.com
Skype: gangsteel18
MSN: gangsteel18@hotmail.com

Tags: A387 Grade 11 Cl1  A387 Grade 11 Cl2  A387 Grade 22 Cl1  A387 Grade 22 Cl2 steel plate  

0 Comments, 0 Trackbacks