New Products /back


ABS EH36,ABS Grade EH36,AB EH36,EH36 steel plate

2011年3月15日 by admin

 

ABS EH36,AB/EH36,EH36 steel,AB/EH36 steel,EH36 steel plate,EH36 grade,abs
 
 
 
Henan Gang iron and steel co., Ltd supply steel grade ABS AH36, ABS DH36, ABS EH36, ABS FH36, ABS AH32, ABS DH32, ABS EH32, ABS FH32, ABS GRADE A, ABS GRADE B, ABS GRADE D, ABS GRADE E. ABS AH40, ABS DH40, ABS EH40, ABS FH40.
 
 
In EH36 steel plate, our mill have more ingot to provide super thick steel plate, our max per weight of plate is above 24.5mt now, max width is 4000mm..
 
EH36 steel grade is lower than FH36 in yield and tensile strength. It is a good material for shipbuilding in deck. EH36 Grade is in -40 impact test of 34J energy. All of thickness of EH36 material need normalize in delivery station.
 
 
Henan Gang iron and steel co., Ltd has exported large thickness is 160mm in this grade to Malaysia shipyard.
 
Henan Gang iron and steel co., Ltd supply EH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.
 
About EH36 detail information,please check technical date in following.
 
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
 EH36
0.180
0.1-0.5
0.90-1.6
0.035
0.035
0.05-0.10
0.015
0.200
Cu %
Mo %
Nb %
Ni %
Ti %
 
 
 
0.350
0.080
0.02-0.05
0.400
0.020
 
 
 

 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
EH36
8mm-50mm
Min 355Mpa
490-620Mpa
21%
-40
 34J
51mm-70mm
Min 355Mpa
490-620Mpa
21%
-40
 41J
71mm-100mm
Min 355Mpa
490-620Mpa
21%
-40
 50J
The min impact energy is longitudinal energy

 
 
Our mill EH36 always be exported to Singapore and Thailand shipyard for shipbuilding.
If you have any need in EH36 steel plate, please feel free to contact us soon.
 
 
ABS EH36,AB/EH36,EH36 steel,AB/EH36 steel,EH36 steel plate,EH36 grade,abs
 
 
Henan Gang iron and steel Co., Ltd
Export Department: Mr. David
Email: david@gangsteel.com
Skype: Gangsteel001
Tel: 86-371-88884766
Fax: 86-371-88884766
Website: www.gangsteel.com
 

Tags: ABS EH36  AB/EH36  EH36 steel  AB/EH36 steel  EH36 steel plate  EH36 grade  ABS  

0 Comments, 0 Trackbacks