Gangsteel pass LR inspection EN10025-3 S355NL 200mm steel plate by ESR Technology

2011年8月17日 by admin

Gangsteel pass LR inspection EN10025-3 S355NL 200mm steel plate by ESR Technology

Gangsteel finish the super thick steel grade along with HBIS wuyang mill technology department in 2011-08-10.
Extra thickness EN10025-3 S355NL in 200mm and 250mm.
Gangsteel technoogy department engineer cooperated with HBIS wuyang mill in electroslag remelting to produce high quality steel plate.
200mm S355nl, after finish LR inspection, the tensile strength is 580Mpa.  Yield strength is 480Mpa, -50 impact test is min 160J.