New Products /back


P420ML1,P420ML2, P460M,P460ML1, P460ML2, steel plate ,EN10028-5

2011年4月17日 by admin

P420ML1,P420ML2, P460M,P460ML1, P460ML2, steel plate ,EN10028-5

 

EN 10028-5 steel grade specification is a weldable fine grain steels thermo mechanically rolled pressure steel plate in grade P355M, P355ML1, P355ML2, P420M, P420ML1, P420ML2, P460M, P460ML1 and P460ML2 steel plate grade.

 

1.  Steel Grade:  P355M, P355ML1, P355ML2, P420M, P420ML1, P420ML2, P460M, P460ML1 and P460ML2 steel plate grade.

2.  Supply steel Size: 

 Thickness: 8mm to 200mm
   Width: 1500mm to 4200mm
   Length: 4000mm to 18000mm

3.  Adopt Standard: EN 10028-5

4.  Heat Treatment: Hot Rolled, CR, Normalized, Quenched, Tempering, TMCP, Electroslag Remelting Technical, HIC test.

5.  Delivery Time: 30-40days

6.  Payment Item: 30% TT, or LC and TT.

7.  Steel Services: Cutting, Painting, Ball blast, Pretreatment , and The third party inspection in DNV, BV, LR, GL, ABS, CCS , CE Mark, TUV, ISO, and others in super thick ship steel plate.

Henan Gang Iron and Steel Co Ltd, is a largest agent of Wuyang mill in HBIS. We have many stock in steel plate stock in shanghai and Wuyang warehouse. 
Gangsteel is specialized in super thick boiler steel plate and cooperated with ABS, BV, DNV, CCS, GL, LR, KR, NK, and RINA Classification Society to approve the super thickness plate to 200mm now.

 

Besides that, Gangsteel Boss is a manufacture manger, so we could promise the delivery time and the competitive price comparing with other company.

We sincerely hope new and old customers come to visit our mill and inquiry from Gangsteel.

 

 

Henan Gang Iron and Steel Co., Ltd

MSN: gangsteel001@hotmail.com

Email: David@gangsteel.com

Skype: gangsteel001

Tel: 86-371-88884766

Web: http://www.gangsteel.com

Tags: P420ML1  P420ML2  P460M  P460ML1  P460ML2  steel plate  EN10028-5  

0 Comments, 0 Trackbacks