New Products /back


S690Q,S690QL, S690QL1, S890Q, S890QL, steel plate, EN10025-6

2011年4月17日 by admin

S690Q,S690QL, S690QL1, S890Q, S890QL, steel plate, EN10025-6

EN 10025-6 steel grade specification is a high yield strength structural steels in the quenched and tempered condition steel plate grade in S500QL, S500QL1, S460Q, S460QL, S460QL1, S620QL1, S550Q, S550QL, S550QL1, S500Q, S890QL1, S960Q, S960QL, S620Q, S620QL, S690Q, S690QL, S690QL1, S890Q and S890QL steel plate grade.

 

1.  Steel Grade:  
S500QL, S500QL1, S460Q, S460QL, S460QL1, S620QL1, S550Q, S550QL, S550QL1, S500Q, S890QL1, S960Q, S960QL, S620Q, S620QL, S690Q, S690QL, S690QL1, S890Q and S890QL steel plate grade.

 2.  Supply steel Size: 

 

   Thickness: 8mm to 300mm
   Width: 1500mm to 4200mm
   Length: 4000mm to 18000mm
3.  Adopt Standard: EN 10025-6
4.  Heat Treatment: Hot Rolled, CR, Normalized, Quenched, Tempering, TMCP, Electroslag Remelting Technical, HIC test.
5.  Delivery Time: 30-40days
6.  Payment Item: 30% TT, or LC and TT.
7.  Steel Services: Cutting, Painting, Ball blast, Pretreatment , and The third party inspection in DNV, BV, LR, GL, ABS, CCS , CE Mark, TUV, ISO, and others in super thick ship steel plate.

Henan Gang Iron and Steel Co Ltd, is a largest agent of Wuyang mill in HBIS. We have many stock in steel plate stock in shanghai and Wuyang warehouse. 
Gangsteel is specialized in super thick low alloy, high strength steel plate and cooperated with ABS, BV, DNV, CCS, GL, LR, KR, NK, and RINA Classification Society to approve the super thickness plate to 300mm now.

 

Besides that, Gangsteel Boss is a manufacture manger, so we could promise the delivery time and the competitive price comparing with other company.

We sincerely hope new and old customers come to visit our mill and inquiry from Gangsteel.

Henan Gang Iron and Steel Co., Ltd

MSN: gangsteel001@hotmail.com

Email: David@gangsteel.com

Skype: gangsteel001

Tel: 86-371-88884766

Web: http://www.gangsteel.com

Tags: S690Q  S690QL  S690QL1  S890Q  S890QL  steel plate  EN10025-6  

0 Comments, 0 Trackbacks