SM520,SM570 ,SM490A, SM490B ,SM490C, steel plate, JIS G3106

 

JIS G3106 steel grade specification is for low alloy high strength steel in steel grade of SM400A, SM400B, SM400C, SM490A, SM490B, SM490C, SM490YB, SM520B, SM520C and SM570 steel grade.

 

1.  Steel Grade: SM400A, SM400B, SM400C, SM490A, SM490B, SM490C, SM490YB, SM520B, SM520C and SM570 steel grade.

 2.  Supply steel Size: 

   Thickness: 8mm to 300mm
   Width: 1500mm to 4200mm
   Length: 4000mm to 18000mm
3.  Adopt Standard: JIS G3106

4.  Heat Treatment: Hot Rolled, CR, Normalized, Quenched, Tempering, TMCP, Electroslag RemeltingTechnical, HIC test.

5.  Delivery Time: 30-40days
6.  Payment Item: 30% TT, or LC and TT.

7.  Steel Services: Cutting, Painting, Ball blast, Pretreatment , and The third party inspection in DNV, BV, LR, GL, ABS, CCS , CE Mark, TUV, ISO, and others in super thick ship steel plate.

Henan Gang Iron and Steel Co Ltd, is a largest agent of Wuyang mill in HBIS. We have many stock in steel plate stock in shanghai and Wuyang warehouse. 


Gangsteel is specialized in super thick low alloy, high strength steel plate and cooperated with ABS, BV, DNV, CCS, GL, LR, KR, NK, and RINA Classification Society to approve the super thickness plate to 300mm now.

Besides that, Gangsteel Boss is a manufacture manger, so we could promise the delivery time and the competitive price comparing with other company.

We sincerely hope new and old customers come to visit our mill and inquiry from Gangsteel.

 

HenanGang Iron and Steel Co., Ltd

Cell: 86-15226033579

Tel: 86-0371-55830820  Fax: 86-0371-88884766
Email: olina@gangsteel.com
Skype: gangsteel18
MSN: gangsteel18@hotmail.com

Gmail: gangsteel18@gmail.com 

Tags: SM520  SM570  SM490A  SM490B  SM490C  steel plate  JIS G3106  

0 Comments, 0 Trackbacks