Steel Category: Low alloy structural steel plate
Adopt standard: A573/ A 573M-05
Sell steel grade: A573 Grade 58, A573 Grade 65 and A573 Grade 70 grade

A573 Gr. 65 Steel Plate
 
 
 
A573 Gr.65 steel is a improved toughness carbon steel plate. The upper limit of manganese for Gr.58 may be exceeded, provided that the carbon content plus 1/6 manganese content does not exceed 0.40% based on heat analysis.

 
If you need more yield and tensile strength in A573 specification, you could choose our steel grade in A573 Gr.70.

 
Gangsteel always exported that A573 Gr.65 steel plate to middle of East Europe country for structural building in bridge and skyscraper.
 
Masteel has cooperated with COSCO ship agent to delivery our goods in bulk ship or containers ship in the fastest delivery to promise time for our customers
 
About A573 Gr.65 steel grade more property, please refer to them in following:
 
 
Table for Chemical list:
 

Grade
C %
Si %
Mn %
P %
S %
A573 Gr.65
0.260
0.15-0.40
0.85-1.2
0.035
0.040

 
 
 
 
Table for yield and tensile strength list:
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
A573 Gr.65
6mm-40mm
240Mpa
450-530Mpa
23%
40mm-100mm
The min impact energy is longitudinal energy

 
 
About the stock specification, because Gangsteel exported all of goods which we ordered for our customers, so we do not have stock goods in A573 Grade 58, A573 Grade 65 and A573 Grade 70 steel plate.
 

If you need A 573 Gr. 65 steel plates, Gangsteel suggest you order them in our mill.
 