Steel Category: Low alloy structural steel plate
Adopt standard: A573/ A 573M-05
Sell steel grade: A573 Grade 58, A573 Grade 65 and A573 Grade 70 steel grade
A573 Gr. 70 steel plate
A573 Gr. 70 steel grade is max yield and tensile in A573 improved toughness carbon steel plate.
A573 Gr.70 usual max thickness is 40mm, in order to satisfy our customers requirement, Gangsteel also could research and development more thick steel plates
If you want a lower yield and tensile grade in A573 specification, you could choose our steel grade in A573 Gr.65 and A573 Gr.58 steel grade.
Gangsteel has cooperated with COSCO ship agent to delivery our goods in bulk ship or containers ship in the fastest delivery to promise time for our customers
Gangsteel sincerely hope old and new customers visit our mill to contact our long steel business in order to enlarge our oversea steel market.
About A573 Gr.70 steel grade more property, please refer to them in following:
Table for Chemical list:
Grade | C % | Si % | Mn % | P % | S % |
A573 Gr.70 | 0.280 | 0.15-0.40 | 0.85-1.2 | 0.035 | 0.040 |
Table for yield and tensile strength lsit:
Grade | Thickness(mm) | Min Yield (Mpa) | Tensile(MPa) | Elongation(%) |
A573 Gr.70 | 6mm-40mm | 290Mpa | 485-620Mpa | 21% |
40mm-100mm | … | … | … | |
The min impact energy is longitudinal energy |
About the stock specification, because Gangsteel exported all of goods which we ordered for our customers, so we do not have stock goods in A573 Grade 70, A573 Grade 65 and A573 Grade 58 steel grade.
If you need A 573 Gr.70 steel plates, Gangsteel suggest you order them in our mill.