AB/DQ70  Extra high Strength Chemical Composition in Tempering and Quenching

Grade

The Element Max (%)

C

Si

Mn

P

S

N

AB/DQ70

0.20

0.55

1.7

0.030

0.030

0.02

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/DQ70 Extra high strength property in tempering and quenching

Grade

Mechanical Property

Charpy V Impact Test

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

Min Mpa

Mpa

Min  %

-20

J

J

AB/DQ70

690

770-940

14

41

62

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of AB/DQ70

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV D690

GL-D690

LR/DH69

BV/D690

CCS/D690

K D70

R D70

RI/D690

 

 

  To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

 

 

 

Tags: ABS DQ70  AB/ DQ70  ABS Grade DQ70  ABS Gr DQ70  AB/ DQ70 steel plate  DQ70 steel grade  

0 Comments, 0 Trackbacks