New Products /back


ABS EH32|AB/EH32 STEEL PLATE

2013年8月22日 by admin

Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade EH32. For more information of GradeEH32 steel plate, please check them in following:

 

AB/EH32 high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

AB/EH32

0.18

0.1-0.50

0.90-1.6

0.035

0.035

0.015

 

Nb

V

Ti

Cu

Cr

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.2

0.4

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/EH32 high strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

AB/EH32

mm

Min Mpa

Mpa

Min  %

0

J

J

t≤50

315

440-590

22%

22

31

50t≤70

315

440-590

22%

26

38

70t≤100

315

440-590

22%

31

46

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

 

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

  

Equivalent steel grade of AB/EH32

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV E32

GL-E32

LR/EH32

BV/EH32

CCS/E32

K E32

R E32

RI/E32

 

  To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

 

 

 

Tags: ABS EH32  AB/ EH32  ABS Grade EH32  ABS Gr EH32  AB/ EH32 steel plate  EH36 steel grade  