Henan Gang iron and steel co., Ltd supply steel grade AB/AH36, AB/DH36, AB/EH36, AB/FH36, AB/AH32, AB/DH32, AB/EH32, AB/FH32, ABS GRADE A, ABS GRADE B, ABS GRADE D, ABS GRADE E. AB/AH40, AB/DH40, AB/EH40, AB/FH40.
In usual if DH32 steel plate thickness above 40mm, mill request the normalized in hot rolled plate, if above 150mm thickness our mill also could use the electroslag remelting technical to do for our customers.
DH32 steel plate usual be used in ship contracture and oil platform. Our mill could produce size in the following:
Thickness: 6mm to 240mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.
Henan Gang iron and steel co., Ltd also could supply super thick steel plate which beyond nine classification society approval.
Henan Gang iron and steel co., Ltd has a strong relationship between with our mill. We could sell DH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.
We sincerely hope old and new customers to visit our mill for a long steel business
About DH32 detail information,please refer to technical date in following.
The Chemical is max composition of product analysis:
Grade | C % | Si % | Mn % | P % | S % | V % | AL % | Cr % |
DH32 | 0.180 | 0.1-0.5 | 0.90-1.6 | 0.035 | 0.035 | 0.05-0.10 | 0.015 | 0.200 |
Cu % | Mo % | Nb % | Ni % | Ti % | | | | |
0.350 | 0.080 | 0.02-0.05 | 0.400 | 0.020 | | | |
The mechanical properties at ambient temperature for quenched and tempered steel plate
Grade | Thickness(mm) | Min Yield (Mpa) | Tensile(MPa) | Elongation(%) | Min Impact Energy | |
DH32 | 8mm-50mm | Min 315Mpa | 440-590Mpa | 22% | -20 | 34J |
51mm-70mm | Min 315Mpa | 440-590Mpa | 22% | -20 | 38J | |
71mm-100mm | Min 315Mpa | 440-590Mpa | 22% | -20 | 46J | |
The min impact energy is longitudinal energy |
If you have any need in DH32 steel plate, please feel free to contact us soon. We sincerely hope old and new customers to visit our mill for a long steel business
Henan Gang iron and steel Co., Ltd
Export Department: Mr. David
Export Department: Mr. David
Email: david@gangsteel.com
Skype: Gangsteel001
Tel: 86-371-88884766
Skype: Gangsteel001
Tel: 86-371-88884766
Fax: 86-371-88884766
Website: www.gangsteel.com
0 Comments, 0 Trackbacks