Henan Gang iron and steel co., Ltd supply steel grade ABS AH36, ABS DH36, ABS EH36, ABS FH36, ABS AH32, ABS DH32, ABS EH32, ABS FH32, ABS GRADE A, ABS GRADE B, ABS GRADE D, ABS GRADE E. ABS AH40, ABS DH40, ABS EH40, ABS FH40.
 
 
 
ABS DH36 steel plate usual be used in ship contracture and oil platform. Our mill could produce size in the following:

Thickness: 6mm to 180mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.
 
Henan Gang iron and steel co., Ltd also could supply super thickness plate which beyond nine classification society approval.
 
Henan Gang iron and steel co., Ltd has a strong relationship between with our mill. We could sell DH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.

 
Henan Gang iron and steel co., Ltd sincerely invite old and new customers to visit our mill for long steel business
 
 
About DH36 detail information,please refer to technical date in following.
 
The Chemical is max composition of product analysis:
 

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
 DH36
0.180
0.1-0.5
0.90-1.6
0.035
0.035
0.05-0.10
0.015
0.200
Cu %
Mo %
Nb %
Ni %
Ti %
 
 
 
0.350
0.080
0.02-0.05
0.400
0.020
 
 
 

 
 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
DH36
8mm-50mm
Min 355Mpa
490-620Mpa
21%
-20
 34J
51mm-70mm
Min 355Mpa
490-620Mpa
21%
-20
 41J
71mm-100mm
Min 355Mpa
490-620Mpa
21%
-20
 50J
The min impact energy is longitudinal energy

 
 
 
Our mill DH36 always be exported to Singapore and Thailand shipyard for shipbuilding.
If you have any need in DH36 steel plate, please feel free to contact us soon.
 
 
Henan Gang iron and steel Co., Ltd
Export Department: Mr. David
Email: david@gangsteel.com
Skype: Gangsteel001
Tel: 86-371-88884766
Fax: 86-371-88884766
Website: www.gangsteel.com
 

Tags: AB DH36  DH36  ABS DH36  Grade DH36  ABS DH36 STEEL  DH36  ABS DH40  

0 Comments, 0 Trackbacks