New Products /back


ABS E,AB/E,ABS Grade E, Grade E steel plate

2011年3月29日 by admin

ABS E,AB/E,ABS Grade E, Grade E steel plate

 

Adopt Standard: ABS Society classification

ABS steel grade:

AB/A

AB/B

AB/D

AB/E

AB/AH32

AB/DH32

AB/EH32

AB/FH32

AB/AH36

AB/DH36

AB/EH36

AB/FH36

AB/AH40

AB/DH40

AB/EH40

AB/FH40

DNV

ABS

LR

BV

 

ABS E steel grade and E steel grade specification:
Thickness: 6mm to 240mm,
Width: 1500mm to 4020mm

Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, Z15, Z25, Z35
UT test: S0E1, S1E2, S2E3 and other standard which be required by customers.

 

Gangsteel is specialized at super thick steel plate which beyond nine classification society approval. We have cooperated with LR, DNV, CCS, ABS, BV, GL, NK, KR, and RINA to do the third party inspection to promise quality for our customers in many years.

 

Gangsteel exported ABS Grade E steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

 

We sincerely hope old and new customers to visit our mill for a long steel business

About ABS E detail information, please refer to technical date in following:

 

ABS Grade E Chemical composition heat analysis

Element

ABS E  Max %

Element

ABS E  max %

C

0.21

Ni

 

Mn

0.60

Mo

 

Si

0.1-0.35

   Al

 

S

0.035

   Nb

 

P

0.035

V

 

Cu

 

Ti

 

    Cr

 

N

 

           

ABS Grade E Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

ABS E

8-240

235

400-520

22

27J

Note: the impact energy under less 50mm thickness

 

If you have any need in ABS Grade E steel plate, please feel free to contact us soon to get a competitive price.

 

Tags: ABS E  Grade E  ABS Grade E  

0 Comments, 0 Trackbacks