AB/EH32,EH32,ABS EH32,EH32 steel,AB/EH32 steel,ABS EH32 steel,EH32,EH40 steel plate
2011年3月9日 by admin
AB/EH32,EH32,ABS EH32,EH32 steel,AB/EH32 steel,ABS EH32 steel,EH32,EH40 steel plate
Henan Gang iron and steel co., Ltd supply steel grade AB/AH36, AB/DH36, AB/EH36, AB/FH36, AB/AH32, AB/DH32, AB/EH32, AB/FH32, ABS GRADE A, ABS GRADE B, ABS GRADE D, ABS GRADE E. AB/AH40, AB/DH40, AB/EH40, AB/FH40.
In EH32 steel plate, our mill have more ingot to provide super thick steel plate, our max per weight of plate is above 24.5mt now, max width is 4000mm..
EH32 steel grade is lower than FH32 in yield and tensile strength. It is a good material for shipbuilding in deck. EH32 Grade is in -40 impact test of 34J energy. All of thickness of EH32 material need normalize in delivery station.
Henan Gang iron and steel co., Ltd supply EH32 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.
Henan Gang iron and steel co., Ltd sincerely invite old and new customers to visit our mill for a long steel business.
About EH32 detail information,please check technical date in following.
The Chemical is max composition of product analysis:
Grade | C % | Si % | Mn % | P % | S % | V % | AL % | Cr % |
EH32 | 0.180 | 0.1-0.5 | 0.90-1.6 | 0.035 | 0.035 | 0.05-0.10 | 0.015 | 0.200 |
Cu % | Mo % | Nb % | Ni % | Ti % | | | | |
0.350 | 0.080 | 0.02-0.05 | 0.400 | 0.020 | | | |
The mechanical properties at ambient temperature for quenched and tempered steel plate
Grade | Thickness(mm) | Min Yield (Mpa) | Tensile(MPa) | Elongation(%) | Min Impact Energy | |
EH32 | 8mm-50mm | Min 315Mpa | 440-590Mpa | 22% | -40 | 34J |
51mm-70mm | Min 315Mpa | 440-590Mpa | 22% | -40 | 38J | |
71mm-100mm | Min 315Mpa | 440-590Mpa | 22% | -40 | 46J | |
The min impact energy is longitudinal energy |
Our mill EH32 always be exported to Singapore and Thailand shipyard for shipbuilding.
If you have any need in EH32 steel plate, please feel free to contact us soon.
Henan Gang iron and steel co., Ltd sincerely invite old and new customers to visit our mill for a long steel business.
Henan Gang iron and steel Co., Ltd
Export Department: Mr. David
Export Department: Mr. David
Email: david@gangsteel.com
Skype: Gangsteel001
Tel: 86-371-88884766
Skype: Gangsteel001
Tel: 86-371-88884766
Fax: 86-371-88884766
Website: www.gangsteel.com
0 Comments, 0 Trackbacks