AB/FH36,ABS FH36,FH36,FH36 steel,AB/FH36 steel plate, Grade FH36,ship steel
2011年3月9日 by admin
AB/FH36,ABS FH36,FH36,FH36 steel,AB/FH36 steel plate, Grade FH36,ship steel
Henan Gang iron and steel co., Ltd supply steel grade AB/AH36, AB/DH36, AB/EH36, AB/FH36, AB/AH32, AB/DH32, AB/EH32, AB/FH32, ABS GRADE A, ABS GRADE B, ABS GRADE D, ABS GRADE E. AB/AH40, AB/DH40, AB/EH40, AB/FH40.
FH36 is a high strength ship steel grade, in -60 charpy V impact and normalized delivery station for construal of ship. Usual max thickness is 100mm, but Our company professional also could provide super thick steel plate Which is beyond Classification Society Authenticate.
Henan Gang iron and steel co., Ltd keeps a long cooperation with nine classification society to let them approval super thickness plates in our mill test certificate.
Henan Gang iron and steel co., Ltd had produced thickness is 110mm in this grade.
Henan Gang iron and steel co., Ltd supply FH36 plates directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.
About FH36 detail information,please check technical date in following.
The Chemical is max composition of product analysis:
Grade | C % | Si % | Mn % | P % | S % | V % | AL % | Cr % |
FH36 | 0.160 | 0.10-0.5 | 0.9-1.6 | 0.025 | 0.025 | 0.05-0.10 | 0.015 | 0.200 |
Cu % | Mo % | Nb % | Ni % | Ti % | N % | | | |
0.350 | 0.080 | 0.02-0.05 | 0.080 | 0.020 | 0.012 | | |
The mechanical properties at ambient temperature for quenched and tempered steel plate
Grade | Thickness(mm) | Min Yield (Mpa) | Tensile(MPa) | Elongation(%) | Min Impact Energy | |
FH36 | 8mm-50mm | Min 355Mpa | 490-620Mpa | 21% | -60 | 34J |
51mm-70mm | Min 355Mpa | 490-620Mpa | 21% | -60 | NA | |
71mm-100mm | Min 355Mpa | 490-620Mpa | 21% | -60 | NA | |
The min impact energy is longitudinal energy |
Our mill FH36 always be exported to Singapore and Thailand shipyard for shipbuilding.
To get our competitive quotation, please feel free to contact us.
Henan Gang iron and steel Co., Ltd
Export Department: Mr. David
Export Department: Mr. David
Email: david@gangsteel.com
Skype: Gangsteel001
Tel: 86-371-88884766
Skype: Gangsteel001
Tel: 86-371-88884766
Fax: 86-371-88884766
Website: www.gangsteel.com
0 Comments, 0 Trackbacks