New Products /back


ABS DH32,AB/DH32,ABS Grade DH32,DH32 steel plate

2011年3月29日 by admin

ABS DH32,AB/DH32,ABS Grade DH32,DH32 steel plate

 

Adopt Standard: ABS Society classification

ABS steel grade:

AB/A

AB/B

AB/D

AB/E

AB/DH32

AB/DH32

AB/EH32

AB/FH32

AB/AH36

AB/DH36

AB/EH36

AB/FH36

AB/AH40

AB/DH40

AB/EH40

AB/FH40

DNV

ABS

LR

BV

 

ABS DH32 steel grade and DH32 steel grade specification:
Thickness: 6mm to 240mm,
Width: 1500mm to 4020mm

Length: 3000mm to 27000mm.
the max weight is 36MT/PCS. In Z test, Z15, Z25, Z35
UT test: S0E1, S1E2, S2E3 and other standard which be required by customers.

 

Gangsteel is specialized at super thick steel plate which beyond nine classification society approval. We have cooperated with LR, DNV, CCS, ABS, BV, GL, NK, KR, and RINA to do the third party inspection to promise quality for our customers in many years.

 

Gangsteel exported ABS DH32 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

 

We sincerely hope old and new customers to visit our mill for a long steel business

About ABS DH32 detail information, please refer to technical date in following:

 

ABS DH32 Chemical composition heat analysis

Element

ABS DH32 Max %

Element

ABS DH32 max %

C

0.18

Ni

0.40

Mn

0.90-1.60

Mo

0.08

Si

0.50

   Al

  0.015 min

S

0.035

   Nb

0.20-0.05

P

0.035

V

0.05-0.10

Cu

0.35

Ti

0.02

    Cr

0.20

N

 

           

ABS DH32 Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-20 degree

ABS DH32

8-240

315

440-590

22

34J

Note: the impact energy under less 50mm thickness

 