AB/AH36 STEEL PLATE

2013年8月23日 by admin

 

 

 Gangsteel is specialized in supplying ABS extra high strength steel plate in ABS AH36 For more information of ABS AH36 steel plate, please check them in following:

 

ABS AH36 extra high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

AB/AH36

0.18

0.10-0.50

0.9-1.6

0.035

0.035

0.015-0.08

 

Nb

V

Ti

Cu

B

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.20

0.40

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

DAB AH36 extra high general strength property

Grade

 

 

Mechanical Property

 

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

AB/AH36

mm

Min Mpa

Mpa

Min  %

0

J

J

t≤50

355

490-620

21%

24

34

50t≤70

355

490-620

21%

27

41

70t≤150

355

490-620

21%

34

50

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

 

Equivalent steel grade of AB/AH36

DNV

KR

LR

BV

CCS

NK

GL

RINA

NV/AH36

R AH36

LR/AH36

BV/AH36

CCS/AH36

K AH36

GL-AH36

RI/AH36

 

 

 To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

 

Tags: ABS AH36  AB/ AH36  ABS Grade AH36  ABS Gr AH36  AB/ AH36 steel plate  ABS Grade AH36 supplier  