New Products /back


AB/DH36, ABS DH36 STEEL PLATE

2013年8月22日 by admin

Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade DH36. For more information of GradeDH36 steel plate, please check them in following:

 

AB/DH36 high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

AB/DH36

0.18

0.1-0.50

0.90-1.6

0.035

0.035

0.015

 

Nb

V

Ti

Cu

Cr

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.2

0.4

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/DH36 high strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

AB/DH36

mm

Min Mpa

Mpa

Min  %

-20

J

J

t≤50

355

490-620

21%

24

34

50t≤70

355

490-620

21%

27

41

70t≤100

355

490-620

21%

34

50

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of AB/DH36

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV D36

GL-D36

LR/DH36

BV/DH36

CCS/D36

K D36

R D36

RI/D36

  

To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

Tags: ABS DH36  AB/ DH36  ABS Grade DH36  ABS Gr DH36  AB/ DH36 steel plate  DH36 steel grade  