AB/DH40,ABS DH40 STEEL PLATE
2013年8月22日 by admin
Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade DH40. For more information of GradeDH40 steel plate, please check them in following:
AB/DH40 high Strength Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
AB/DH40 | 0.18 | 0.1-0.50 | 0.90-1.6 | 0.035 | 0.035 | 0.015 | |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
AB/DH40 high strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
AB/DH40 | mm | Min Mpa | Mpa | Min % | 0 | J | J |
t≤50 | 390 | 510-650 | 20% | 26 | 39 | ||
50<t≤70 | 390 | 510-650 | 20% | 31 | 46 | ||
70<t≤100 | 390 | 510-650 | 20% | 37 | 55 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
Equivalent steel grade of AB/DH40 | |||||||
NV D40 | GL-D40 | LR/DH40 | BV/DH40 | CCS/D40 | K D40 | R D40 | RI/D40 |
To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.
Tags: ABS DH40 AB/ DH40 ABS Grade DH40 ABS Gr DH40 AB/ DH40 steel plate DH40 steel grade