Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade DQ43. For more information of Grade DQ43 steel plate, please check them in following:

 

AB/DQ43  Extra high Strength Chemical Composition in Tempering and Quenching

Grade

The Element Max (%)

C

Si

Mn

P

S

N

AB/DQ43

0.20

0.55

1.7

0.030

0.030

0.02

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/DQ43 Extra high strength property in tempering and quenching

Grade

Mechanical Property

Charpy V Impact Test

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

Min Mpa

Mpa

Min  %

-20

J

J

AB/DQ43

420

530-680

18

27

41

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of AB/DQ43

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV D420

GL-D420

LR/DH42

BV/D420

CCS/D420

K D43

R D43

RI/D420

 

To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

Tags: ABS DQ43  AB/ DQ43  ABS Grade DQ43  ABS Gr DQ43  AB/ DQ43 steel plate  DQ43 steel grade  

0 Comments, 0 Trackbacks