ABS DQ63|AB/DQ63 STEEL PLATE
2013年8月22日 by admin
Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade DQ63. For more information of Grade DQ63 steel plate, please check them in following:
AB/DQ63 Extra high Strength Chemical Composition in Tempering and Quenching | ||||||
Grade | The Element Max (%) | |||||
C | Si | Mn | P | S | N | |
AB/DQ63 | 0.20 | 0.55 | 1.7 | 0.030 | 0.030 | 0.02 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
AB/DQ63 Extra high strength property in tempering and quenching | ||||||
Grade | Mechanical Property | Charpy V Impact Test | ||||
Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
Min Mpa | Mpa | Min % | -20 | J | J | |
AB/DQ63 | 620 | 720-890 | 15 | 41 | 62 | |
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
Equivalent steel grade of AB/DQ63 | |||||||
NV D620 | GL- D620 | LR/DH62 | BV/D620 | CCS/D620 | K D63 | R D63 | RI/D620 |
To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.