AB/EH36|ABS EH36 STEEL PLATE
2013年8月22日 by admin
Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade EH36. For more information of GradeEH36 steel plate, please check them in following:
AB/EH36 high Strength Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
AB/EH36 | 0.18 | 0.1-0.50 | 0.90-1.6 | 0.035 | 0.035 | 0.015 | |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
AB/EH36 high strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
AB/EH36 | mm | Min Mpa | Mpa | Min % | 0 | J | J |
t≤50 | 355 | 490-620 | 21% | 24 | 34 | ||
50<t≤70 | 355 | 490-620 | 21% | 27 | 41 | ||
70<t≤100 | 355 | 490-620 | 21% | 34 | 50 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
Equivalent steel grade of AB/EH36 | |||||||
NV E36 | GL-E36 | LR/EH36 | BV/EH36 | CCS/E36 | K E36 | R E36 | RI/E36 |