AB/EH40|ABS EH40 STEEL PLATE

2013年8月22日 by admin

Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade EH40. For more information of GradeEH40 steel plate, please check them in following:

 

AB/EH40 high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

AB/EH40

0.18

0.1-0.50

0.90-1.6

0.035

0.035

0.015

 

Nb

V

Ti

Cu

Cr

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.2

0.4

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/EH40 high strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

AB/EH40

mm

Min Mpa

Mpa

Min  %

0

J

J

t≤50

390

510-650

20%

26

39

50t≤70

390

510-650

20%

31

46

70t≤100

390

510-650

20%

37

55

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of AB/EH40

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV E40

GL-E40

LR/EH40

BV/EH40

CCS/E40

K E40

R E40

RI/E40

 

To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

Tags: ABS EH40  AB/EH40  ABS Grade EH40  ABS Gr EH40  AB/EH40 steel plate  EH40 steel grade  