New Products /back


AB/EQ43|ABS EQ43 STEEL PLATE

2013年8月22日 by admin

Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade EQ43. For more information of Grade EQ43 steel plate, please check them in following:

 

AB/EQ43  Extra high Strength Chemical Composition in Tempering and Quenching

Grade

The Element Max (%)

C

Si

Mn

P

S

N

AB/EQ43

0.20

0.55

1.7

0.030

0.030

0.02

 Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/EQ43 Extra high strength property in tempering and quenching

Grade

Mechanical Property

Charpy V Impact Test

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

Min Mpa

Mpa

Min  %

-20

J

J

AB/EQ43

420

530-680

18

27

41

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of AB/EQ43

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV E420

GL-E420

LR/EH42

BV/E420

CCS/E420

K E43

R E43

RI/E420

 

To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

Tags: ABS EQ43  AB/EQ43  ABS Grade EQ43  ABS Gr EQ43  AB/EQ43 steel plate  EQ43 steel grade  

0 Comments, 0 Trackbacks