New Products /back


AB/EQ51|ABS EQ51 STEEL PLATE

2013年8月21日 by admin

Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade EQ51. For more information of Grade EQ51 steel plate, please check them in following:

 

AB/EQ51  Extra high Strength Chemical Composition in Tempering and Quenching

Grade

The Element Max (%)

C

Si

Mn

P

S

N

AB/EQ51

0.20

0.55

1.7

0.030

0.030

0.02

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/EQ51 Extra high strength property in tempering and quenching

Grade

Mechanical Property

Charpy V Impact Test

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

Min Mpa

Mpa

Min  %

-40

J

J

AB/EQ51

500

610-770

16

33

50

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of AB/EQ51

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV E500

GL-E500

LR/EH50

BV/E500

CCS/E500

K E51

R E51

RI/E500

 

To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

Tags: ABS EQ51  AB/EQ51  ABS Grade EQ51  ABS Gr EQ51  AB/EQ51 steel plate  EQ51 steel grade  