AB/EQ56|ABS EQ56 STEEL PLATE
2013年8月21日 by admin
Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade EQ56. For more information of Grade EQ56 steel plate, please check them in following:
AB/EQ56 Extra high Strength Chemical Composition in Tempering and Quenching | ||||||
Grade | The Element Max (%) | |||||
C | Si | Mn | P | S | N | |
AB/EQ56 | 0.20 | 0.55 | 1.7 | 0.030 | 0.030 | 0.02 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
AB/EQ56 Extra high strength property in tempering and quenching | ||||||
Grade | Mechanical Property | Charpy V Impact Test | ||||
Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
Min Mpa | Mpa | Min % | -40 | J | J | |
AB/EQ56 | 550 | 670-835 | 16 | 37 | 55 | |
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
Equivalent steel grade of AB/EQ56 | |||||||
NV E550 | GL-E550 | LR/EH55 | BV/E550 | CCS/E550 | K E56 | R E56 | RI/E550 |
To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.
Tags: AB/EQ56 ABS EQ56 ABS Grade EQ56 AB/EQ56 steel plate ABS Gr EQ56 EQ56 steel grade