New Products /back


AB/EQ63 |ABS EQ63 STEEL PLATE

2013年8月21日 by admin

Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade EQ63. For more information of Grade EQ63 steel plate, please check them in following:

 

AB/EQ63  Extra high Strength Chemical Composition in Tempering and Quenching

Grade

The Element Max (%)

C

Si

Mn

P

S

N

AB/EQ63

0.20

0.55

1.7

0.030

0.030

0.02

 

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/EQ63 Extra high strength property in tempering and quenching

Grade

Mechanical Property

Charpy V Impact Test

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

Min Mpa

Mpa

Min  %

-40

J

J

AB/EQ63

620

720-890

15

41

62

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

 Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of AB/EQ63

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV E620

GL- E620

LR/EH62

BV/E620

CCS/E620

K E63

R E63

RI/E620

 

 To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

 

 

 

Tags: ABS EQ63  AB/EQ63  ABS Grade EQ63  ABS Gr EQ63  AB/EQ63 steel plate  EQ63 steel grade  

0 Comments, 0 Trackbacks