Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade FH32. For more information of GradeFH32 steel plate, please check them in following:

 

AB/FH32 high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

AB/FH32

0.16

0.1-0.50

0.90-1.6

0.025

0.025

0.015

0.009

Nb

V

Ti

Cu

Cr

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.2

0.8

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/FH32 high strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

AB/FH32

mm

Min Mpa

Mpa

Min  %

-60

J

J

t≤50

315

440-590

22%

22

31

50t≤70

315

440-590

22%

26

38

70t≤100

315

440-590

22%

31

46

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of AB/FH32

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV F32

GL-F32

LR/FH32

BV/FH32

CCS/F32

K F32

R F32

RI/F32

 

 To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

 