New Products /back


AB/FH36|ABS FH36 STEEL PLATE

2013年8月20日 by admin

Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade FH36. For more ``information of GradeFH36 steel plate, please check them in following:

 

AB/FH36 high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

AB/FH36

0.16

0.1-0.50

0.90-1.6

0.025

0.025

0.015

0.009

Nb

V

Ti

Cu

Cr

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.2

0.8

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/FH36 high strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

AB/FH36

mm

Min Mpa

Mpa

Min  %

-60

J

J

t≤50

355

490-620

21%

24

34

50t≤70

355

490-620

21%

27

41

70t≤100

355

490-620

21%

34

50

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of AB/FH36

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV FH36

GL-FH36

LR/FH36

BV/FH36

CCS/FH36

K FH36

R FH36

RI/FH36

 

 To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

 

Tags: ABS FH36  AB/FH36  ABS Grade FH36  FH36 Steel Grade  AB/FH36 steel plate  ABS Gr.FH36  

0 Comments, 0 Trackbacks