AB/FH40|ABS FH40 STEEL PLATE

2013年8月20日 by admin

Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade FH40. For more information of GradeFH40 steel plate, please check them in following:

 

AB/FH40 high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

AB/FH40

0.16

0.1-0.50

0.90-1.6

0.025

0.025

0.015

0.009

Nb

V

Ti

Cu

Cr

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.2

0.8

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/FH40 high strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

AB/FH40

mm

Min Mpa

Mpa

Min  %

-60

J

J

t≤50

390

510-650

20%

26

39

50t≤70

390

510-650

20%

31

46

70t≤100

390

510-650

20%

37

55

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

Equivalent steel grade of AB/FH40

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV F32

GL-F32

LR/FH40

BV/FH40

CCS/F32

K F32

R F32

RI/F32

 

 To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

Tags: AB/FH40  ABS FH40  ABS Garde FH40  ABS Gr FH40  AB/FH40 steel plate  ABS steel grade  

0 Comments, 0 Trackbacks