AB/FQ47|ABS FQ47 STEEL PLATE

2013年8月20日 by admin

 

Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade FQ47. For more information of Grade FQ47 steel plate, please check them in following:

 

AB/FQ47  Extra high Strength Chemical Composition in Tempering and Quenching

Grade

The Element Max (%)

C

Si

Mn

P

S

N

AB/FQ47

0.18

0.55

1.60

0.025

0.025

0.02

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

AB/FQ47 Extra high strength property in tempering and quenching

Grade

Mechanical Property

Charpy V Impact Test

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

Min Mpa

Mpa

Min  %

-40

J

J

AB/FQ47

460

570-720

17

31

46

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate

 

 

 

Equivalent steel grade of AB/FQ47

DNV

GL

LR

BV

CCS

NK

KR

RINA

NV F460

GL-F460

LR/FH46

BV/F460

CCS/F460

K F47

R F47

RI/F460

 

 To find out more information for shipbuilding steel plate, and receive a competitive quotation, please CLICK HERE to contact us or click our warehouse sizes.

 

 

Tags: ABS FQ47  AB/FQ47  ABS Grade FQ47  ABS FQ47 steel plate  AB/FQ47 steel grade  ABS Gr FQ47  

0 Comments, 0 Trackbacks