New Products /back


ABS Grade E shipbuilding steel plate

2013年8月16日 by admin

ABS Grade E shipbuilding steel plate

 
 
Gangsteel is specialized in supplying ABS general strength steel plate in ABS Grade E. For more information of Grade E steel plate, please check them in following:
 
 

ABS GRADE E general Strength Chemical Composition
Grade
The Element Max (%)
C
Si
Mn
P
S
N
ABS GRADE E
0.18
0.1-0.35
0.70
0.035
0.035
0.02

Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
 
 
 

ABS GRADE general strength property
Grade
 
Mechanical Property
Charpy V Impact Test
Thickness
Yield
Tensile
Elongation
Degree
Energy 1
Energy 2
ABS GRADE E
mm
Min Mpa
Mpa
Min %
-40
J
J
t≤50
235
400-520
22%
20
27
50<t≤70
235
400-520
22%
24
34
70<t≤100
235
400-520
22%
27
41
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
 
 
 
 

Equivalent steel grade of ABS GRADE E
NV E
GL-E
LR/E
BV/E
CCS/E
K E
R E
RI/E

 
 
 
If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.
 
 
 

Tags: ABS Grade E  ABS Gr.E  ABS GRE  ABS Gr.E steel grade  ABS Grade E supplier  