New Products /back


EQ56,ABS EQ56,AB/EQ56,AB/EQ56,steel plate

2011年4月13日 by admin

EQ56,ABS EQ56,AB/EQ56,AB/EQ56,steel plate

 

Related mill: HBIS (heibei iron & steel co.,ltd),Wisco (wuhan iron and steel group),Shougang mill (shougang group), Xinyu mill (xinyu iron & steel co., ltd),Baosteel (Baosteel group co.,ltd)

 

Keyword:EQ56,ABS EQ56,AB/EQ56,AB/EQ56 ship steel,EQ56 steel,EQ56 price,EQ56 steel plate, abs grade EQ56.

ABS Grade EQ56 Detail productive technology in the following:

 

1.       Adopt standard: ABS (American Bureau of shipping)

2.       EQ56 application fields:
EQ56 is a super high strength quenched and tempered steel grade. It used in offshore drilling platform, Shipping marine engineering and Hull Structural project.

3.       EQ56 Chemical composition:

 

Grade

C % max

Si % max

Mn % max

P % max

S % max

AB/EQ56

0.20

0.55

1.70

0.030

0.030

 

4.       EQ56 Mechanical Property:

  

Grade

Yield Strength

Tensile Strength

Elongation

Impact Energy

ABS EQ56

MPa (min)

MPa

% (min)

-40 degree J

AB/EQ56

 550

670-835

16

55

 

5.       Heat Treatment: Quenched and tempered


6.  Tolerance: The thickness tolerance is -+0.03mm


7.  Size: Thick: 8mm-180mm, width: 1500mm-4000mm, length: 3000mm-18000mm

 

8.        Delivery time: 40-45days

 

Gangsteel has much experience in super high strength hull structural steel plate, if you have any need in ABS/EQ56 steel plate; please feel free to contact us. We will give our mill competitive price on the base of faster delivery.

 

Other super strength steel grade in Gangsteel:

ABS Grade A,ABS GRADE B, abs grade d, abs grade e, abs grade ah36, abs grade dh36, abs grade eh36, abs grade fh36, abs grade ah32, abs grade dh32, abs grade eh32, abs grade fh32, abs grade dh40, abs grade eh40, abs grade ah40, abs grade fh40

AB/AQ43,AB/DQ43,AB/EQ43,AB/AQ47,AB/DQ47,AB/EQ47,AB/AQ51,AB/DQ51,AB/EQ51,AB/AQ56,AB/DQ56,AB/EQ56,AB/AQ63,AB/DQ63,AB/EQ63,AB/AQ70,AB/DQ70,AB/EQ70,

 

 

 

Tags: EQ56  ABS EQ56  AB EQ56  AB EQ56  steel plate  

0 Comments, 0 Trackbacks