FQ56,ABS FQ56,AB/FQ56,AB/FQ56,steel plate

2011年4月13日 by admin

FQ56,ABS FQ56,AB/FQ56,AB/FQ56,steel plate

 

Related mill: HBIS (heibei iron & steel co.,ltd),Wisco (wuhan iron and steel group),Shougang mill (shougang group), Xinyu mill (xinyu iron & steel co., ltd),Baosteel (Baosteel group co.,ltd)

 

Keyword:FQ56,ABS FQ56,AB/FQ56,AB/FQ56 ship steel,FQ56 steel,FQ56 price,FQ56 steel plate, abs grade FQ56.

ABS Grade FQ56 Detail productive technology in the following:

 

1.       Adopt standard: ABS (American Bureau of shipping)

2.       FQ56 application fields:
FQ56 is a super high strength quenched and tempered steel grade. It used in offshore drilling platform, Shipping marine engineering and Hull Structural project.

3.       FQ56 Chemical composition:

 

Grade

C % max

Si % max

Mn % max

P % max

S % max

AB/FQ56

0.18

0.55

1.60

0.025

0.025

 

4.       FQ56 Mechanical Property:

  

Grade

Yield Strength

Tensile Strength

Elongation

Impact Energy

ABS FQ56

MPa (min)

MPa

% (min)

-60 degree J

AB/FQ56

 550

670-835

16

55

 

5.       Heat Treatment: Quenched and tempered


6.  Tolerance: The thickness tolerance is -+0.03mm


7.  Size: Thick: 8mm-180mm, width: 1500mm-4000mm, length: 3000mm-18000mm

 

8.        Delivery time: 40-45days

 

Gangsteel has much experience in super high strength hull structural steel plate, if you have any need in ABS/FQ56 steel plate; please feel free to contact us. We will give our mill competitive price on the base of faster delivery.

 

Other super strength steel grade in Gangsteel:

AB/AQ43,AB/DQ43,AB/EQ43,AB/AQ47,AB/DQ47

AB/EQ47,AB/FQ56,AB/DQ51,AB/EQ51,AB/FQ56,

AB/DQ56,AB/EQ56,AB/AQ63,AB/DQ63,AB/EQ63,

AB/AQ70,AB/DQ70,AB/EQ70

 

 

 

 

Tags: FQ56  ABS FQ56  AB FQ56  AB FQ56  steel plate  

0 Comments, 0 Trackbacks