New Products /back


FQ63,ABS FQ63,AB/FQ63,AB/FQ63,steel plate

2011年4月13日 by admin

FQ63,ABS FQ63,AB/FQ63,AB/FQ63,steel plate

 

Related mill: HBIS (heibei iron & steel co.,ltd),Wisco (wuhan iron and steel group),Shougang mill (shougang group), Xinyu mill (xinyu iron & steel co., ltd),Baosteel (Baosteel group co.,ltd)

 

Keyword:FQ63,ABS FQ63,AB/FQ63,AB/FQ63 ship steel,FQ63 steel,FQ63 price,FQ63 steel plate, abs grade FQ63.

ABS Grade FQ63 Detail productive technology in the following:

 

1.       Adopt standard: ABS (American Bureau of shipping)

2.       FQ63 application fields:
FQ63 is a super high strength quenched and tempered steel grade. It used in offshore drilling platform, Shipping marine engineering and Hull Structural project.

3.       FQ63 Chemical composition:

 

Grade

C % max

Si % max

Mn % max

P % max

S % max

AB/FQ63

0.18

0.55

1.60

0.025

0.025

 

4.       FQ63 Mechanical Property:

  

Grade

Yield Strength

Tensile Strength

Elongation

Impact Energy

ABS FQ63

MPa (min)

MPa

% (min)

-60 degree J

AB/FQ63

 620

720-890

15

62

 

5.       Heat Treatment: Quenched and tempered


6.  Tolerance: The thickness tolerance is -+0.03mm


7.  Size: Thick: 8mm-180mm, width: 1500mm-4000mm, length: 3000mm-18000mm

 

8.        Delivery time: 40-45days

 

Gangsteel has much experience in super high strength hull structural steel plate, if you have any need in ABS/FQ63 steel plate; please feel free to contact us. We will give our mill competitive price on the base of faster delivery.

 

Other super strength ABS steel grade in Gangsteel:

AB/AQ43,AB/DQ43,AB/EQ43,AB/AQ47,AB/DQ47,

AB/EQ47,AB/AQ51,AB/DQ51,AB/EQ51,AB/AQ56,

AB/DQ56,AB/EQ56,AB/FQ63,AB/DQ63,AB/EQ63

,AB/AQ70,AB/DQ70,AB/EQ70

 

 

 

Tags: FQ63  ABS FQ63  AB FQ63  AB FQ63  steel plate  

0 Comments, 0 Trackbacks