New Products /back


ABS FH32,AB/FH32,FH32 steel,AB/FH32 steel,ABS FH32 steel,FH32,steel plate

2011年3月9日 by admin

 

 ABS FH32,AB/FH32,FH32 steel,AB/FH32 steel,ABS FH32 steel,FH32,steel plate
 
 
 
Henan Gang iron and steel co., Ltd supply steel grade AB/AH36, AB/DH36, AB/EH36, AB/FH36, AB/AH32, AB/DH32, AB/EH32, AB/FH32, ABS GRADE A, ABS GRADE B, ABS GRADE D, ABS GRADE E. AB/AH40, AB/DH40, AB/EH40, AB/FH40.
 
 
 
FH32 is a high strength ship steel grade, in normalized delivery station for construal of ship. Usual max thickness is 100mm, but Our company professional also could provide super thick steel plate Which is beyond Classification Society Authenticate.
 
 
Henan Gang iron and steel co., Ltd keeps a long cooperation with nine classification society to let them approval super thickness plates in our mill test certificate.

 
We have produced thickness is 140mm in this grade.
 
Henan Gang iron and steel co., Ltd supply FH32 plates directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.
 
 
 
About FH32 detail information,please check technical date in following.
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
FH32
0.160
0.10-0.5
0.9-1.6
0.025
0.025
0.05-0.10
0.015
0.200
Cu %
Mo %
Nb %
Ni %
Ti %
N %
 
 
0.350
0.080
0.02-0.05
0.080
0.020
0.012
 
 

 
 
 
 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
FH32
8mm-50mm
Min 315Mpa
440-590Mpa
22%
-60
 34J
51mm-70mm
Min 315Mpa
440-590Mpa
22%
-60
 NA
71mm-100mm
Min 315Mpa
440-590Mpa
22%
-60
 NA

 
 
 
 
Our mill FH32 always be exported to Singapore and Thailand shipyard for shipbuilding.
To get our competitive quotation, please feel free to contact us.
 
 
Henan Gang iron and steel Co., Ltd
Export Department: Mr. David
Email: david@gangsteel.com
Skype: Gangsteel001
Tel: 86-371-88884766
Fax: 86-371-88884766
Website: www.gangsteel.com

Tags: ABS FH32  FH32  FH32 steel  ABS FH32  ABS FH32 steel  FH32  steel plate  

0 Comments, 0 Trackbacks