New Products /back


ah36 steel | ah36 steel plate

2011年8月30日 by admin

ah36 steel | ah36 steel plate

Henan Gang iron and steel co., Ltd supply steel grade ABS AH36, ABS DH36, ABS EH36, ABS FH36, ABS AH32, ABS DH32, ABS EH32, ABS FH32, ABS GRADE A, ABS GRADE B, ABS GRADE D, ABS GRADE E. ABS AH40, ABS DH40, ABS EH40, ABS FH40.
 
 
 
In usual if AH36 steel plate thickness above 50mm, mill request the normalized in hot rolled plate Or control rolled, if above 150mm thickness our mill also could use the electroslag remelting technical in ingot to do for our customers.
 
 
AH36 steel plate usual be used in ship contracture and oil platform. Our mill could produce size in the following:

Thickness: 6mm to 300mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.
 
Henan Gang iron and steel co., Ltd also could supply super thick steel plate thickness from 100mm to 300mm which beyond nine classification society approval.
 
 Henan Gang iron and steel co., Ltd has a strong relationship between with our mill. We could sell DH36 steel material directly in our mill cost price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.

We sincerely hope old and new customers to visit our mill for a long steel business
 
 
About AH36 detail information,please refer to technical date in following.
The Chemical is max composition of product analysis:
 

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
 AH36
0.180
0.1-0.5
0.90-1.6
0.035
0.035
0.05-0.10
0.015
0.200
Cu %
Mo %
Nb %
Ni %
Ti %
 
 
 
0.350
0.080
0.02-0.05
0.400
0.020
 
 
 

 
 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
AH36
8mm-50mm
Min 355Mpa
490-620Mpa
21%
0
 34J
51mm-70mm
Min 355Mpa
490-620Mpa
21%
0
 41J
71mm-100mm
Min 355Mpa
490-620Mpa
21%
0
 50J
The min impact energy is longitudinal energy

 
 
 
If you have any need ABS AH36 steel plate, please feel free to contact us soon. We sincerely hope old and new customers to visit our mill for a long steel business
 
 
ABS AH36,AB/AH36,AH36 steel,AB/AH36 steel, AH36 steel plate,AH36 grade
 
 