New Products /back


ASME SA203 Grade B|SA203 Gr.B STEEL PLATE

2011年6月10日 by admin

ASME SA203 Grade B|SA203 Gr.B STEEL PLATE

ASME SA203 Grade B steel grade is a nickel alloy steel plate in welded pressure vessels. For this SA203 Grade B is max thickness in 150mm and the element of nickel is 2.25% to be used in manufacturing pressure vessel and boilers.

 

ASME SA203 Grade B is used in fabricators serving industry, especially in the oil, gas and chemical supply markets.

 

Our plates including SA203 Gr.B come with mill certificate in accordance with EN 10204 3.1 or EN 10204 3.2. We welcome any third party or customer inspection if required.

 

Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 |

 

Dimension: Thickness: 6MM to 150MM,

Width: 1500mm to 4050mm,

Length: 3000mm to 15000mm
 

Gangsteel is specialized in supplying ASME SA203 steel plate in SA203 Grade B. For more information of SA203 Grade B steel plates, please check them in following:

 

SA203 Grade B Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

SA203 Grade B

0.17

0.13-0.45

0.78-0.88

0.035

0.035

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Mechanical Property of SA203 Grade B steel plate

SA203 Grade B

Tensile strength, kis [MPa]

70-90[485-620]

Yield strength, min, kis [MPa]

40 [275]

Elongation in 8 in. [200 mm], min, %

17

Elongation in 2 in. [50 mm], min, %

21

Shipbuilding steel plate | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

  

Related Grade: SA203 Grade A|SA203 Grade D| SA203 Grade E | SA203 Grade F

Tags: SA203 Gr.B  SA203 Grade B  A203 grade B  ASME SA203 Gr.B  SA203 Gr.B steel  

0 Comments, 0 Trackbacks