New Products /back


SA203 Gr.F|SA203 Grade F steel plate

2013年9月4日 by admin

SA203 Grade F steel plate

 

SA203 Grade F steel is the element of nickel is 3.25% to be used in manufacturing pressure vessel and boilers steel grade. SA203 Gr.F steel plate should be heated by heating into the austenitic range, quenching in water and tempering at not less than 1100 degree for not less than 30 minutes.

 

The max thickness is 100mm. if you need more thickness, Gangsteel also could supply for our customers. We also could do the third party inspection in CCS, BV, ABS, LR, KR, GL, DNV, CE, and others to promise the quality for our long cooperation.

 

Steel plate SA203 Grade F, compare with SA203 Grade A, SA203 Grade B, SA203 Grade D, and SA203 Grade E, the yield and tensile strength is the highest to 380Mpa and 550Mpa. That is better in weld ability to boiler steel and vessel.

 

Gangsteel has much experience exporting boiler plate in SA203 Grade F to factory mill many years. Besides that, Gangsteel has a specialized person who worked at production line of steel, to arrange our customer goods to produce as early as possible. Gangsteel welcomes our customer to visit in our mill.

SA203 Grade F steel Chemical Requirements In product analysis under 50mmthickness

Element

SA203 Grade A  Max %

C

0.20

Si

0.13-0.45

Mn

0.78-0.88

P

0.035

S

0.035

Ni

3.18-3.82


 

SA203 Grade F steel Tensile Requirements:
 

SA203 Grade F

Tensile strength, kis [MPa]

50mmor under

Over 50mm

 

Yield strength, min, kis [MPa]

50mmor under

Over 50mm
Elongation in 8 in. [200 mm], min, %
Elongation in 2 in. [50 mm], min, %

Tensile strength, kis [MPa]

80-100 [550-690]
75-95  [515-655]

Yield strength, min, kis [MPa]

55 [380]

50 [345]

…..

20


 

If you have any need in SA203 Grade F, please contact Gangsteel soon by email or calling.

 

Tags: SA203 Grade F  SA203 Gr.F  SA203 GRF  SA203 Gr.F steel plate  ASME SA203 Gr.F  ASME SA203 Gr.F  ASME SA203 Grade F  SA203 GRF supplier  SA203 Grade F steel grade  SA203 Gr.F price  SA203 Grade F  

0 Comments, 0 Trackbacks